Aka-Clear-2 Powder

Polvo para sistema acrílico bicomponente de curado rápido para montajes transparentes. Ideal para el análisis de fallos y en la preparación de componentes electrónicos gracias a la completa visibilidad de la muestra.

Cura en 7 – 8 min a temperatura ambiente. Temperatura de pico 85 – 89 ℃.

Mezclar 2 – 2,5 partes de polvo con 1 parte de líquido (en volumen). La vida útil es de 1 – 2 min y la dureza es de 85 – 87 Shore D.

Descripción

Contenido disponible: 1 kg, 5 kg

Aka-Clear 2 Guías del usuario

FDS Aka-Clear-2 Polvo

Información adicional

Contenido disponible

1 kg, 5 kg

  • Akasel Aka-NoStick Liquid in a clear plastic bottle with a white screw cap. The label features the product name "Aka-NoStick Liquid" and the description "Water-based mould release liquid for easy extracting of cold-setting mounts." Additional information: Contents 250 ml, Item No. 25901201 (8420), made in Denmark. Specially developed for metallographic applications to guarantee effortless sample removal during cold mounting.

    Embutición

    Aka-NoStick Liquid

  • Akasel Aka-Mould: Dark blue cold mounting mold with a smooth, round inner surface, shown from above. The heat- and chemical-resistant mold is specially designed for metallographic applications and is compatible with all cold mounting materials. It is used as a two-part system. Available sizes: 25 mm, 30 mm, 40 mm, 50 mm.

    Embutición

    Aka-Mould

  • Akasel Aka-Clear-2 Liquid, 500 ml: Brown glass bottle with a yellow cap holding liquid for a two-component acrylic system. The label displays the product name, Item No. 25202413 (8602), as well as information on fast curing and specific usage instructions. Specially developed for metallographic applications, perfect for producing transparent mounts when used with Aka-Clear-2 Powder for accurate analysis and sample preparation.

    Embutición en frío - Metalografía

    Aka-Clear-2 Liquid

  • Akasel Cold Mounting Mixing Kit – Cups Stacked: Stack of turquoise mixing cups displaying the Akasel logo and the slogan "The Smarter Alternative" on the front. A QR code with the text "Scan for instruction videos" is prominently displayed. Multiple wooden sticks extend from the top cup. Specially designed for metallographic cold mounting processes, compatible with all cold mounting materials.

    Embutición

    Cold Mounting Mixing Kit

Contáctenos