Aka-Mono+ 3 µm

High concentration monocrystalline diamond suspension for metallographic sample preparation.
Recommended for all materials, but ideal for hard materials.

Aka-Mono+ ensures the fastest preparation possible with outstanding removal rates. Provides the possibility of precise adjustment of diamond suspension/lubricant ratio.

Diamond concentration of 40 ct/l

100% monocrystalline diamonds
Median (50%) 2.84 µm
Tolerance 2.7 – 2.98 µm
Upper limit (99%) 4.1 µm

Keep out of direct sunlight.

Additional information

Content available

500 ml, 1 l, 2.5 l