Aka-Mono 9 µm

Monocrystalline diamond suspension for metallographic sample preparation.
Recommended for all materials.

Aka-Mono is an economical diamond suspension that provides fast sample preparation and the possibility of precise adjustment of diamond suspension/lubricant ratio.

Diamond concentration of 20 ct/l
100% monocrystalline diamonds
Median (50%) 9.6 µm
Tolerance 9.12 – 10.08 µm
Upper limit (99%) 12.9 µm

Keep out of direct sunlight.

Additional information

Content available

500 ml, 1 l, 2.5 l, 5 l